S31803/S32205
Short Description:
Introduction Stainless steels are high-alloy steels. These steels are available in four groups that include martensitic, austenitic, ferritic and precipitation-hardened steels. These groups are formed based on the crystalline structure of stainless steels. Stainless steels contain larger amounts of chromium in comparison with other steels and thus have good corrosion resistance. Most of the stainless steels contain about 10% of chromium. Grade 2205 stainless steel is a duplex stainless st...
Product Detail
FAQ
Product Tags
IntroductionStainless steels are high-alloy steels. These steels are available in four groups that include martensitic, austenitic, ferritic and precipitation-hardened steels. These groups are formed based on the crystalline structure of stainless steels. Stainless steels contain larger amounts of chromium in comparison with other steels and thus have good corrosion resistance. Most of the stainless steels contain about 10% of chromium. Grade 2205 stainless steel is a duplex stainless steel whose design enables combining improved resistance to pitting, high strength, stress corrosion, crevice corrosion and cracking. Grade 2205 stainless steel resists sulfide stress corrosion and chloride environments. The following datasheet provides an overview of grade 2205 stainless steel. Chemical CompositionThe chemical composition of grade 2205 stainless steel is outlined in the following table.
Physical PropertiesThe following table shows the physical properties of grade 2205 stainless steel.
Mechanical PropertiesThe mechanical properties of grade 2205 stainless steel are displayed in the following table.
Thermal PropertiesThe thermal properties of grade 2205 stainless steel are given in the following table.
Other DesignationsEquivalent materials to grade 2205 stainless steel are:
Fabrication and Heat TreatmentAnnealingGrade 2205 stainless steel is annealed at 1020-1070°C (1868-1958°F) and then water quenched. Hot WorkingGrade 2205 stainless steel is hot worked in the temperature range of 954-1149°C (1750-2100°F). Hot working of this grade stainless steel under room temperature is recommended whenever possible. WeldingWelding methods recommended for grade 2205 stainless steel include SMAW, MIG, TIG and manual covered electrode methods. During the welding process, the material should be cooled below 149°C (300°F) between passes and preheating of the weld piece should be avoided. Low heat inputs should be used for welding grade 2205 stainless steel. FormingGrade 2205 stainless steel is difficult to form due to its high strength and work hardening rate. MachinabilityGrade 2205 stainless steel can be machined with either carbide or high speed tooling. The speed is reduced by about 20% when carbide tooling is used. ApplicationsGrade 2205 stainless steel is used in the following applications:
|