Kovar / Nilo K (ASTM F15)
Short Description:
Technical Data Sheet Kovar Chemical Composition (Basic Density 8.36) Weight % Ni Fe Co C Mn Si Al Cr Mg Zr Ti Cu Mo Alloy K Kovar 29.0 53.0 17.0 0.04 max 0.50 max 0.20 0.10 max 0.20 max 0.10 max 0.10 max 0.10 max 0.20 max 0.20 max Kovar (Alloy K) is a nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, matches the expansion rate of borosilicate glasses and alumina ceramics...
Product Detail
FAQ
Product Tags
Technical Data Sheet
Kovar Chemical Composition (Basic Density 8.36) | |||||||||||||
Weight % | Ni | Fe | Co | C | Mn | Si | Al | Cr | Mg | Zr | Ti | Cu | Mo |
Alloy K Kovar |
29.0 | 53.0 | 17.0 | 0.04 max | 0.50 max | 0.20 | 0.10 max | 0.20 max | 0.10 max | 0.10 max | 0.10 max | 0.20 max | 0.20 max |
Kovar (Alloy K) is a nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, matches the expansion rate of borosilicate glasses and alumina ceramics. Kovar (Alloy K) is used for glass-to-metal seals in applications requiring high reliability or resistance to thermal shock. Kovar (Alloy K) is used for high-power transmitting valves, transistor leads and headers, integrated-circuit lead frames, and photography flash bulbs.
Typical Mechanical Properties
Material | Condition | Yield Strength (0.1% Offset) | Tensile Strength | Elongation % | ||
psi | MPa | psi | MPa | |||
Alloy K Kovar |
Annealed | 49,000 | 340 | 75,000 | 520 | 42 |
Availability
Alloy K / Kovar is available (further details) in Bar, Rod, Tube, Sheet, Strip, Coil, Plate and Wire. For all stock availability contact Sales for further availability.
Specifications
UNS K94610
Werkstoff Nr 1.3981
DIN 17745
ASTM F 15
AMS 7726 Wire
AMS 7727 Bars and Forgings
AMS 7728 Sheet, Strip and Plate
MIL-I-23011 class 1
AFNOR NF A54-301
S.E.W 385
DILVER P